A satellite in low Earth orbit circles the planet roughly every 90 minutes, and its solar panels alternately heat up in full sunlight and cool down in the planet's shadow. In November 2026 the issue made the news again: the Chinese company Yanhe Technology sent three perovskite-based photovoltaic modules into orbit, one of them flexible, which will be tested, among other things, during thermal cycling. We explain why temperature changes load the adhesive layer under the cells, why its flexibility matters, and what the parameters of the WACKER® RTV-S 691 A/B silicone say about it.
Some sixteen day–night cycles every day
With one orbit roughly every 90 minutes, a satellite completes about 16 orbits a day and about 6,000 a year. NASA engineers quoted this figure when designing the solar arrays for the Freedom space station, and they also noted temperature swings of more than 160 °C. For the panels of the Hubble Space Telescope, in turn, the requirement was to withstand 30,000 thermal cycles over five years, in a range from about +100 to −100 °C.
The number and length of eclipses, however, depend on the orbit. According to pv magazine (14 November), one of the Yanhe satellites, North University of China-1, flies in a dawn–dusk orbit, where the Sun shines almost without interruption. Nothing in that article indicates which adhesives were used in the Yanhe modules.
What happens in the adhesive layer
A solar cell is a thin wafer covered with a cover glass and bonded to the panel substrate. Each of these materials expands differently: the coefficient of thermal expansion is about 2.6 for silicon, about 8.5 for glass and about 23 for aluminium (in units of 10⁻⁶ per kelvin, at 20 °C). For specific cover glasses and substrates the values differ, but the differences remain.
With temperature changes of around 200 °C, the differences in expansion turn into shear stresses in the adhesive layer. Repeated thousands of times, these stresses can lead to glass cracking, delamination and damaged joints. A 1965 NASA report on cover-glass adhesives already pointed this out: in thermal shock and vibration tests, rigid epoxy adhesives caused the glass to crack, while silicone ones, thanks to their flexibility, caused no serious cracking.
An adhesive's flexibility at low temperatures is determined by its glass transition temperature (Tg). Below it, an elastomer becomes stiff and brittle, so if the adhesive cooled down in Earth's shadow below its own Tg, it would stop absorbing the differences in contraction of the cell, the glass and the substrate. That is why Tg should lie well below the lowest operating temperature.
How RTV-S 691 A/B fits in
WACKER® RTV-S 691 A/B is a self-levelling, two-component, addition-curing silicone rubber that vulcanises at room temperature (RTV-2). It was developed as an adhesive for solar cells on solar generators in satellites. It has a glass transition temperature below −100 °C and stays flexible at low temperatures, and once cured its elongation at break is 100–160% at a hardness of 50–60 Shore A. It is also resistant to high temperature and UV radiation. ESTEC (the European Space Research and Technology Centre) has approved it for aerospace applications under specification ECSS-Q-70-02A, and its particularly low content of volatile substances matters for optics and cells in a vacuum.
The mixing ratio of components A and B is 9:1 by weight, and the pot life of the mixture is 90–110 minutes. The material can be applied by screen printing or with dispensing equipment. Before application, the mixed RTV-S 691 A/B must be degassed under vacuum to remove entrapped air bubbles, which can weaken the bond. For the rubber to adhere to glass, aluminium, silver and epoxy and polyester resins, prepare the surface beforehand with WACKER® PRIMER G 790 TOLUENE FREE primer. You will find more about primers in the guide Primer G 790 – when to use it and how to apply it correctly.
Also remember that the platinum catalyst is in component A and the crosslinker in component B. Equipment used with component A or with the mixture must therefore not touch component B, and the components should come from the same production batch. The values in this article are indicative and should not be used as a basis for drawing up specifications. The mechanical properties were measured after 5 minutes of pressing at 165 °C and 6 hours of post-curing at 100 °C. The glass transition temperature and flexibility describe the adhesive itself. The behaviour of a panel also depends on layer thickness and on the type of glass and substrate, so it must be verified in tests, including thermal cycling.
Need help choosing?
See the product page for WACKER® RTV-S 691 A/B 1 kg or browse the whole category: RTV-2 two-component silicones. The product price is available on request. If you have any questions, contact us. We will be happy to help.